Zinc Phosphate Process Line
Alkaline Degreasing
Rinsing
Activation
Zinc Phosphating
Passivation
Drying
temp : 70-90 ºC time: 5-15 min. tank : can be DKP.
Ambient Temp.
temp. : 60-70 ºC time : 5-8 min. tank : stainless conical
temp. : 20-60 ºC time : 0.5-2 min. tank : stainless
temp: max.120 ºC